Re: C60 orthorhombic structure

2021-09-24 Thread Alan Hewat
Dear Francois.
I did a quick non-exhaustive search of ICSD for pure C60, and posted the
results on https://neutronoptics.com/downloads/C60-icsd.jpg
This includes claims of tetragonal and orthorhombic structures. You can
search Google with the paper titles to find the references if you don't
have access to ICSD :-) The old neutron powder work I previously referred
to from memory was
Nature (1991) 353, 147-149  *Crystal
structure and bonding of ordered C60*
David, W.I.F.;Ibberson, R.M.;Matthewman, J.C.;Prassides, K.;Dennis,
T.J.S.;Hare, J.P.;Kroto, H.W.;Taylor, R.;Walton, D.R.M.
This paper is copyright by Nature, but have put ICSD details on
https://neutronoptics.com/downloads/C60-icsd_66729.jpg

Below the 249K transition, the structure becomes ordered with a different
cubic phase. You will find more ISIS work on C60 with inclusion compounds,
eespecially superconducting K3C60 on
https://neutronoptics.com/downloads/K-C60-icsd.jpg including Peter
Steven's paper.
Kind Regards, Alan.

On Fri, 24 Sept 2021 at 16:18, Alan Hewat 
wrote:

> Dear Francois.
>
> Thank you for putting the paper on your private server rather than sending
> it to the whole list. However the correct link should be:
> https://perso.univ-lemans.fr/~fgouten/C60/
> Koichi KIKUCHI, et al Physiea C 185-189 (1991) 415-416
> STRUCTURE AND SUPERCONDUCTIVITY OF SINGLE CRYSTALLINE C80
> There are quite a number of papers on C60 superconductors, in particular
> by Bill David and colleagues at ISIS, and it would be worthwhile doing a
> broader search of the literature.
>
> Kind regards, Alan.
>
> On Fri, 24 Sept 2021 at 14:56, francois Goutenoire <
> francois.gouteno...@univ-lemans.fr> wrote:
>
>> Dear Rietveld users,
>>
>> Sorry for the mistake, the paper was published in 1991.
>>
>> I put the paper in the link
>>
>> http:\\perso.univ-lemans.fr\~fgouten\C60
>>
>> From the previous answer it seems that it is not really realiable.
>>
>> Best wishes françois Goutenoire
>>
>>
>> Le 24/09/2021 à 12:05, francois Goutenoire a écrit :
>>
>> Dear Rietveld users,
>>
>> We are currently looking for the atomic structure (cif file) of the C60
>> Orthorhombic cell
>>
>> The previous paper : "Structure and superconductivity of single
>> crystalline C60" from Koichi Kikuchi et al.
>>
>> Physica C in 1975
>>
>> The cell parameters are given  a=25.011 Ang, b=25.582 Ang. c=10.003 Ang.
>> Space group Pbnm
>>
>> but there is not atomic position in the paper.
>>
>> Best regards, françois Goutenoire
>>
>>
>> ++
>> Please do NOT attach files to the whole list  
>> 
>> Send commands to   eg: HELP as the subject 
>> with no body text
>> The Rietveld_L list archive is on 
>> http://www.mail-archive.com/rietveld_l@ill.fr/
>> ++
>>
>>
>> --
>> *
>> Pr. Francois GOUTENOIRE
>> e-mail: francois.gouteno...@univ-lemans.fr
>> Tel: 02.43.83.33.54
>> FAX: 02.43.83.35.06
>> Skype Entreprise visio conférence
>> Département des Oxydes et Fluorures
>> Institut des Molécules et des Matériaux du Mans
>> IMMM - UMR CNRS 6283
>> Université du Maine - Avenue Olivier Messiaen
>> F-72085 Le Mans Cedex 9
>> FRANCE
>> *
>> Formation Rietveld CNRS 
>> 2020https://cnrsformation.cnrs.fr/diffraction-des-rayons-x-sur-materiaux-polycristallins?axe=135
>> Formation EDX CNRS 
>> 2020https://cnrsformation.cnrs.fr/fluorescence-x-edx?axe=135
>> Formation SAXS et Réflectivités pour couches minces et matériaux 
>> nanostructurés.https://cnrsformation.cnrs.fr/caracterisation-des-materiaux-nanostructures-par-diffusion-des-rayons-x?axe=135
>> Bibliographiehttps://scholar.google.fr/citations?hl=fr&user=qC-lmN4J&view_op=list_works&authuser=1&sortby=titlehttps://orcid.org/-0001-5339-3002
>>
>> ++
>> Please do NOT attach files to the whole list > >
>> Send commands to  eg: HELP as the subject with no body
>> text
>> The Rietveld_L list archive is on
>> http://www.mail-archive.com/rietveld_l@ill.fr/
>> ++
>>
>>
>
> --
> __
> *   Dr Alan Hewat, NeutronOptics, Grenoble, FRANCE *
>  +33.476.98.41.68
> http://www.NeutronOptics.com/hewat TVA FR 79499450856
> __
>


-- 
__
*   Dr Alan Hewat, NeutronOptics, Grenoble, FRANCE *
 +33.476.98.41.68
http://www.NeutronOptics.com/hewat TVA FR 79499450856
__
++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as

Re: C60 orthorhombic structure

2021-09-24 Thread Alan Hewat
Dear Francois.

Thank you for putting the paper on your private server rather than sending
it to the whole list. However the correct link should be:
https://perso.univ-lemans.fr/~fgouten/C60/
Koichi KIKUCHI, et al Physiea C 185-189 (1991) 415-416
STRUCTURE AND SUPERCONDUCTIVITY OF SINGLE CRYSTALLINE C80
There are quite a number of papers on C60 superconductors, in particular by
Bill David and colleagues at ISIS, and it would be worthwhile doing a
broader search of the literature.

Kind regards, Alan.

On Fri, 24 Sept 2021 at 14:56, francois Goutenoire <
francois.gouteno...@univ-lemans.fr> wrote:

> Dear Rietveld users,
>
> Sorry for the mistake, the paper was published in 1991.
>
> I put the paper in the link
>
> http:\\perso.univ-lemans.fr\~fgouten\C60
>
> From the previous answer it seems that it is not really realiable.
>
> Best wishes françois Goutenoire
>
>
> Le 24/09/2021 à 12:05, francois Goutenoire a écrit :
>
> Dear Rietveld users,
>
> We are currently looking for the atomic structure (cif file) of the C60
> Orthorhombic cell
>
> The previous paper : "Structure and superconductivity of single
> crystalline C60" from Koichi Kikuchi et al.
>
> Physica C in 1975
>
> The cell parameters are given  a=25.011 Ang, b=25.582 Ang. c=10.003 Ang.
> Space group Pbnm
>
> but there is not atomic position in the paper.
>
> Best regards, françois Goutenoire
>
>
> ++
> Please do NOT attach files to the whole list  
> 
> Send commands to   eg: HELP as the subject 
> with no body text
> The Rietveld_L list archive is on 
> http://www.mail-archive.com/rietveld_l@ill.fr/
> ++
>
>
> --
> *
> Pr. Francois GOUTENOIRE
> e-mail: francois.gouteno...@univ-lemans.fr
> Tel: 02.43.83.33.54
> FAX: 02.43.83.35.06
> Skype Entreprise visio conférence
> Département des Oxydes et Fluorures
> Institut des Molécules et des Matériaux du Mans
> IMMM - UMR CNRS 6283
> Université du Maine - Avenue Olivier Messiaen
> F-72085 Le Mans Cedex 9
> FRANCE
> *
> Formation Rietveld CNRS 
> 2020https://cnrsformation.cnrs.fr/diffraction-des-rayons-x-sur-materiaux-polycristallins?axe=135
> Formation EDX CNRS 
> 2020https://cnrsformation.cnrs.fr/fluorescence-x-edx?axe=135
> Formation SAXS et Réflectivités pour couches minces et matériaux 
> nanostructurés.https://cnrsformation.cnrs.fr/caracterisation-des-materiaux-nanostructures-par-diffusion-des-rayons-x?axe=135
> Bibliographiehttps://scholar.google.fr/citations?hl=fr&user=qC-lmN4J&view_op=list_works&authuser=1&sortby=titlehttps://orcid.org/-0001-5339-3002
>
> ++
> Please do NOT attach files to the whole list  >
> Send commands to  eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/rietveld_l@ill.fr/
> ++
>
>

-- 
__
*   Dr Alan Hewat, NeutronOptics, Grenoble, FRANCE *
 +33.476.98.41.68
http://www.NeutronOptics.com/hewat TVA FR 79499450856
__
++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++



Re: C60 orthorhombic structure

2021-09-24 Thread francois Goutenoire

Dear Rietveld users,

Sorry for the mistake, the paper was published in 1991.

I put the paper in the link

http:\\perso.univ-lemans.fr\~fgouten\C60

From the previous answer it seems that it is not really realiable.

Best wishes françois Goutenoire


Le 24/09/2021 à 12:05, francois Goutenoire a écrit :

Dear Rietveld users,

We are currently looking for the atomic structure (cif file) of the 
C60 Orthorhombic cell


The previous paper : "Structure and superconductivity of single 
crystalline C60" from Koichi Kikuchi et al.


Physica C in 1975

The cell parameters are given  a=25.011 Ang, b=25.582 Ang. c=10.003 
Ang. Space group Pbnm


but there is not atomic position in the paper.

Best regards, françois Goutenoire


++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++


--
*
Pr. Francois GOUTENOIRE
e-mail: francois.gouteno...@univ-lemans.fr
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Skype Entreprise visio conférence
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*
Formation Rietveld CNRS 2020
https://cnrsformation.cnrs.fr/diffraction-des-rayons-x-sur-materiaux-polycristallins?axe=135
Formation EDX CNRS 2020
https://cnrsformation.cnrs.fr/fluorescence-x-edx?axe=135
Formation SAXS et Réflectivités pour couches minces et matériaux nanostructurés.
https://cnrsformation.cnrs.fr/caracterisation-des-materiaux-nanostructures-par-diffusion-des-rayons-x?axe=135
Bibliographie
https://scholar.google.fr/citations?hl=fr&user=qC-lmN4J&view_op=list_works&authuser=1&sortby=title
https://orcid.org/-0001-5339-3002

++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++



C60 orthorhombic structure

2021-09-24 Thread francois Goutenoire

Dear Rietveld users,

We are currently looking for the atomic structure (cif file) of the C60 
Orthorhombic cell


The previous paper : "Structure and superconductivity of single 
crystalline C60" from Koichi Kikuchi et al.


Physica C in 1975

The cell parameters are given  a=25.011 Ang, b=25.582 Ang. c=10.003 Ang. 
Space group Pbnm


but there is not atomic position in the paper.

Best regards, françois Goutenoire

--
*
Pr. Francois GOUTENOIRE
e-mail: francois.gouteno...@univ-lemans.fr
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Skype Entreprise visio conférence
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*
Formation Rietveld CNRS 2020
https://cnrsformation.cnrs.fr/diffraction-des-rayons-x-sur-materiaux-polycristallins?axe=135
Formation EDX CNRS 2020
https://cnrsformation.cnrs.fr/fluorescence-x-edx?axe=135
Formation SAXS et Réflectivités pour couches minces et matériaux nanostructurés.
https://cnrsformation.cnrs.fr/caracterisation-des-materiaux-nanostructures-par-diffusion-des-rayons-x?axe=135
Bibliographie
https://scholar.google.fr/citations?hl=fr&user=qC-lmN4J&view_op=list_works&authuser=1&sortby=title
https://orcid.org/-0001-5339-3002

++
Please do NOT attach files to the whole list 
Send commands to  eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++