After you eliminate the alpha2 using the PowerX, simply save it in GSAS format
by Selecting Save data from the File menu and choose the GSAS .DAT with
PowderX.
Cheng Dong
Dear all,
I have a little problem and hope someone to help me.
After I used the PowerX to remove the eliminate the
yes, i can save in GSAS .DATformat, but i can not import this format into
the GSAS. The software always reminds me it is not the proper format. Can
you give me further advice?
Thanks in advance!
Iris
From: Cheng Dong [EMAIL PROTECTED]
Reply-To: rietveld_l@ill.fr
To: rietveld_l@ill.fr
Have you tried Cnvfile ?
I've never had to use it but I hear it works wonders!
Jo
-Original Message-
From: liu 迎新 [mailto:[EMAIL PROTECTED]
Sent: 03 April 2007 12:03
To: rietveld_l@ill.fr
Subject: Re: about format convert
yes, i can save in GSAS .DATformat, but i can not import this
Excuse me, i have not heard of it. is it a software?
Iris
From: Duncan, Jo [EMAIL PROTECTED]
Reply-To: rietveld_l@ill.fr
To: rietveld_l@ill.fr
Subject: RE: Re: about format convert
Date: Tue, 3 Apr 2007 12:44:29 +0100
Have you tried Cnvfile ?
I've never had to use it but I hear it works
It is an option in GSAS. In PCGSAS: Setup - Cnvfile
jo
-Original Message-
From: liu 迎新 [mailto:[EMAIL PROTECTED]
Sent: 03 April 2007 13:16
To: rietveld_l@ill.fr
Subject: RE: Re: about format convert
Excuse me, i have not heard of it. is it a software?
Iris
From: Duncan, Jo [EMAIL
Hi,
A few important points:
1) Removing Ka2 from the powder pattern is not necessary for running GSAS (or
Fullpoof for that matter). Both represent the Ka1-Ka2 doublet quite nicely.
More important, most Ka2 stripping routines can adversly distort the data
messing up the result from a Rietveld
Thanks a lot! I will think about it carefully.
Iris
From: Von Dreele, Robert B. [EMAIL PROTECTED]
Reply-To: rietveld_l@ill.fr
To: rietveld_l@ill.fr
Subject: RE: RE: RE: Re: about format convert
Date: Tue, 3 Apr 2007 07:52:43 -0500
Hi,
A few important points:
1) Removing Ka2 from the