Hi,everyone
Who knew the atom fractional coordinates of Li2SnO3.
Please tell me. Thanks in advance.
Best regards,
Hansan Liu
The State Key Lab for Physical
Chemistry of the Solid Surface,
Xiamen University,P.R.China
E-mail:[EMAIL PROTECTED]
Hi,everyone
Who knew the atom fractional coordinates of Li2SnO3?
Please tell me. Thanks in advance.
Best regards,
Hansan Liu
The State Key Lab for Physical
Chemistry of the Solid Surface,
Xiamen University,P.R.China
E-mail:[EMAIL PROTECTED]
Who know the atom fractional coordinates of Li2SnO3?
there is some confusion about the correct coordinates in the
old (1954 Lang, Z. Anorg. Allg. Chem.) literature.
the correct values are:
TITL Lithium stannate
TITL Li2 Sn O3 Die Kristallstruktur von Li2SnO3 Kreuzburg G Stewner F Hoppe R
TITL
TITL Li2 Sn O3 Die Kristallstruktur von Li2SnO3 Kreuzburg G Stewner F Hoppe
Actually a more recent paper (using neutron Rietveld refinement :-) is:
Hodeau,JL. Marezio,M. Santoro,A. Roth,RS. (1982) J.Solid State Chem 45 170-179
Neutron Profile Refinement of the Structures of Li2 Sn O3 and Li2 Zr
Dear Dr. Liu: I have handy two reprints about the crystal structure of
Li2SnO3. Data are as follows:
G.Kreuzburg, F. Stewner und R. Hoppe, Z.Anorg.Allg.Chem., v. 379,
pp.242-254,(1970)
S.G. C2/c; a=5.295, b=9.184, c=10.032, beta=100.13 deg., Z=8
Single Crystal XRD data
Atomposition x