Thank every one for the propositions.
Find here after the result of a test (vaseline + n-heptane)
http://perso.univ-lemans.fr/~fgouten/Transmission_Tricks
Best Regards, François
Le 08/02/2017 13:35, François Goutenoire a écrit :
Dear Rietveld users,
We are currently using transmission flat
velaga <vsrihari_k...@yahoo.co.in>
Sent: Thursday, February 9, 2017 12:08:57 AM
To: François Goutenoire; rietveld_l@ill.fr
Subject: Re: Tricks for transmission sample preparation between foils
Dear Pr. Francois GOUTENOIRE,
In case of kapton tape there is a chance of getting diffraction peak at l
Dear Pr. Francois GOUTENOIRE,
In case of kapton tape there is a chance of getting diffraction peak at low
angle, I prefer to use magic scotch tape.
Some times to avoid the background from this tape as well, I use small punch in
the thick paper card and pack the material in that hole for
Dear Rietveld users,
Following Pr. Francois Goutenoire's question, I would like to add another
question: I wonder how do you deal with electrostatic powders sample
preparation though in Reflection mode. Do you use Kapton/mylar tape or any
solvent to disperse the powder?
How does it affect the