> discussion on PPM of CS. You can buy a TDS 1 dissolved solids tester from > Hanna Instruments -- www.hannainst.com for $14.95.
I just ordered mine. So, is there any consensus on the ideal PPM to use? I once heard that 30PPM or greater was best, but with the recent speculation about clumping (or silver oxide formation), I am not so sure. On the last batch, I made a quart with Sota (.9999) wires and 36V. I left it go for a half hour after the cloud began to form. As soon as the cloud started to form and every 6 minutes after, I cleaned the electrodes since this seems to be what causes it to go yellow. It does not taste any stronger or weaker than what I typically produce, which is to let the thing go until it just starts to go yellow without cleaning the electrodes. turf -- The silver-list is a moderated forum for discussion of colloidal silver. To join or quit silver-list or silver-digest send an e-mail message to: [email protected] -or- [email protected] with the word subscribe or unsubscribe in the subject: line. To post, address your message to: [email protected] List maintainer: Mike Devour <[email protected]>