Action Electronics no longer recommends using salt solution.  They use a
starter solution to speed up the making the CS.

Quoting from instructions:  "Since this is the method that Bob Beck is now
recommending and prefers, we will no longer be supplying the sea salt or
dropper bottle as we had previously."

----------
> From: RingDance <[email protected]>
> To: [email protected]
> Subject: Use of salt solution for making CS
> Date: Thursday, January 08, 1998 6:00 PM
> 
> In a recent post to the list I recall that I said that the Beck
instructions
> that I had did not mention adding salt to the distilled water.  In going
> through my files again, I find that I was incorrect and that the
instructions
> received from Action Electronics does mention adding a salt solution to
the
> distilled water.
> 
> Quoting from the instructions:
>  
> "Then place the silver electrode wire into a tall, narrow glass
containing 8
> oz of distilled water and a drop of saturated salt solution.'
> 
> The instructions then go on to say:
> 
> "Making a saturated salt solution for distilled water.  This is made from
pure
> salt such as 'Light Gray Celtic Sea Salt' from the Grain and Salt
Society,
> P.O. Box DD, Magalia, CA 95954.  Do not use table salt as it contains
> additives like iodine, aluminum and silica desiccates.  Mix one and
one-half
> teaspoons of salt in one ounce of distilled water.  Let stand for a few
hours
> and filter off the top liquid.  The salt must be dissolved in water
before
> using.  The salt solution may be stored for repeated use in a 1 oz brown
glass
> dropper bottle.  Add a little silver colloid to this to prevent bacteria
> growth.  Then use only 1 drop of this saline solution each time you make
> silver colloid.  It is important that you do not use excess salt or you
will
> not be making silver colloid but silver chloride. As more salt solution
is
> added, the silver comes off the electrode faster, but the micron size
also
> gets larger.  Using one drop per 8 oz water is the best for making a
particle
> size than can be absorbed more thoroughly.  As little as 4 drops can
change
> the chemical formulation into silver chloride."
> 
> H. Davis