Hi Ya'all;

"Ole Bob" hasn't been on the net much to post just developing a new CS
Gen and reading all of the wierd and wonderful things being posted.

In the process of developing my polarity switching generator several
very interesting things have materialized.
With good water and good silver, polarity switching makes colorless CS
up to at least 35 ppm (26 hours), with no cleaning, treeing, and very
little sludge. Notice that "good silver" is in italics and underlined.
During the development stage I needed to make some new electrodes and
used a new lot of silver.

With good silver the electrodes are a mouse gray but these turned to
coal black. When questioning the supplier I found out that they had
shipped sterling silver. Besides having black electrodes the CS after
three hours was developing a faint hint of color.

It just maybe that a lot of the color problems that you CSers are having
is not using five nine silver.

The second problem is could very easily come from not having a stable
process nor monitoring the current during the formation. A simple
battery and bulb system requires a lot of close monitoring to get a
reliable and repeatable product.

I expect a lot of flack, but how much data have you recorded in your CS
making? I have hundreds of sheets of curves generated during the
developmental process. And since I make my own spectrophotometeric
measurements, and conductive measurements. I know what I have and what
the polarity reversal will do. I have it down to "fill and brew." Time
it with a commercially available lamp timer.

Robert