Hi Bob or CS experts,
Susan here, EE. You mention 35ppm--how--are you using 27V LVDC?

Question for you. OK, so I've made my CS using silver from Marsha online and 
I didn't switch the electrodes. Started with a pint jar. But I've made 1 
quart in a glass jar at a time--I've made a couple gallons so far. When done, 
it is faint yellow (clear) with lots of feathering and eventually major black 
crud on an electode (negative I believe--can't recall). The next AM it is 
clear dark gold. I let it go until 6-6.5mA per my meter (not current 
limited). I kept stirring it until it was consistently 6.5mA--took over an 
hour.

It stains the jar. Anyway, I took this silver and it did nothing compared to 
the 30ppm Source Natural that has been helping. I could tell in a major way 
the two weeks I tried it. So I need to figure how to make it better--it 
appears a bit useless in the form that I am making it.

So what am I doing wrong? Is it that I am not switching the electrodes? Need 
more pure silver? Too much water at a time? Not pure enough distilled H20? 
(Know a good brand?) Do I stir it or just let it go until concentration at 
the 6.5mA is between the 1" electrodes? The electrodes are 5", submersed 4" 
and 1" apart. Do I need to current limit it? If so, how is best? Rheostat or 
resistor or ? My electrodes are black when I wipe them on a tissue--and I 
definitely have to strain with coffee filter due to the black particles from 
the one electrode.

Any idea why the dark gold after 8 hours? Does that indicate large particle 
size?

My doctor claimed he makes it by leaving it only 5 minutes, LVDC---????sounds 
awfully short. Mine doesn't start feathering for 15-20 min.

Thanks for your help,
Susan L

In a message dated 99-07-23 20:05:20 EDT, you write:

<< Hi Ya'all;
 
 "Ole Bob" hasn't been on the net much to post just developing a new CS
 Gen and reading all of the wierd and wonderful things being posted.
 
 In the process of developing my polarity switching generator several
 very interesting things have materialized.
 With good water and good silver, polarity switching makes colorless CS
 up to at least 35 ppm (26 hours), with no cleaning, treeing, and very
 little sludge. Notice that "good silver" is in italics and underlined.
 During the development stage I needed to make some new electrodes and
 used a new lot of silver.
 
 With good silver the electrodes are a mouse gray but these turned to
 coal black. When questioning the supplier I found out that they had
 shipped sterling silver. Besides having black electrodes the CS after
 three hours was developing a faint hint of color.
 
 It just maybe that a lot of the color problems that you CSers are having
 is not using five nine silver.
 
 The second problem is could very easily come from not having a stable
 process nor monitoring the current during the formation. A simple
 battery and bulb system requires a lot of close monitoring to get a
 reliable and repeatable product.
 
 I expect a lot of flack, but how much data have you recorded in your CS
 making? I have hundreds of sheets of curves generated during the
 developmental process. And since I make my own spectrophotometeric
 measurements, and conductive measurements. I know what I have and what
 the polarity reversal will do. I have it down to "fill and brew." Time
 it with a commercially available lamp timer.
 
 Robert
  >>


--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: 
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]

List maintainer: Mike Devour <[email protected]>