The suggestion to put a tiny amount of H202 in the water as an electrolyte is an interesting idea which I will try. In the meantime I have had a lot of success just adhering to the fundamentals: 1- Pyrex gallon jar for production 2- .9999 pure very thin silver wire, as thin and pure as I can buy it. 3- Make electrodes of about 5 feet long wire loosely looped to a twisted loop about 8 inches long about 1/2 inch diameter for both electrodes. 4- Just use the device per directions and you will get a very high quality 20 PPM product.