Hi Bill,

Many experienced makers of CS think the best compromise of simplicity, 
economy and adequate accuracy for measuring PPM/mgL is with wet chemistry 
and a spectrophotometer.  That method is  much more reliable than measuring 
the conductivity of an Ag sol, which has significant variations between 
test instruments and is highly dependent upon calibration procedures.  Most 
who have tried it and checked the results with a spec. see wild variations 
in data.  You might write Bob Berger for his data.

A Spec can easily be checked by testing a precision dilution of a 
 certified silver standard, such as silver nitrate, and the method is 
inherently more stable.

A test for total silver can be done locally by a pro lab for about 30 
dollars, so it is not inaccessible to those who do not wish to set up a 
lab.

Regardless of the total silver in a sol, the parameter of particle size is 
much more important in determining the effectiveness of the sol.  A very 
low concentration of small particles, for example 5 mg/L, being more 
effective than a very high concentration of, for example alleged 500 mg/L. 
Particle size is much more expensive to measure, costing about $150 per 
test,  unless you do quite a few.

James Osbourne Holmes
[email protected]


-----Original Message-----
From:   Hutt William J (Bill) DLPC [SMTP:[email protected]]
Sent:   Wednesday, October 20, 1999 9:23 AM
To:     [email protected]
Subject:        CS ppm standard



     I've read many e-mails on this forum about achieved ppm, but little on 
how the parties accomplished and confirmed their results.  It would be nice
to create a data base of methods in order to create a standard.
I have seen a couple of e-mails which addressed using a volt-ohm-meter
to read ppm.

 Example:  4usec/cm = 1/250kohms;  this measurement appears to be achieved
by placing the VOM probes in the CS solution at a spacing of 1cm.

Example2: 1ppm = 1.6usec/cm (+/- 20%);  If both examples are correct then
5ppm would be equal to 5ppm X 1.6usec/cm = 8usec/cm
 8usec/cm = 1/R = 125kohms resistance between the VOM probes which are
spaced 1cm apart in the CS solution.

If we can gather data from known ppm solutions using the above method ,a
rough standard could be established and everyone would know about what
strength of CS solution they have produced.

Resistance measurements of  5ppm, 10ppm, 20ppm, and 30ppm  should give a
well rounded data base.

I realize that their are many other factors to consider when trying to
measure ppm.  The purpose of this e-mail is to try and establish a standard
by which everyone can use without purchasing some expensive high tech
device.

If a simple standard has already been established, what is it?

     I would like to know if anyone has a recipe for making colloidal 
silver
salve.

                                                 Thank you,

                                                    BillH


--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to:
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]