At 10:28 AM 6/29/2000, you wrote:
I have noticed when I make CS (LVDC method, pure DW, no additives), the
conductivity of the end product drops during the first day. I measure the
conductivity with the Hanna PWT immediately after completing and stirring a
batch, then the next day. Here are some readings to illustrate this. They
are after - next day, in microSeimens: 23.8 - 16.0, 19.2 - 10.5, 22.6 -
16.2, 10.0 - 7.8.
What is going on during the first day to cause the drop in measured
"strength"?
--Steve
I would check it after an hour and 4 hours also. If most drop is in the
first hour you did not mix it well! If a steady drop thru 4 hours and 24
then you have crystals and they are growing (stealing the ions). Is
there any drop after a few days? Make and keep it in glass or plastic?
[email protected]
--
The silver-list is a moderated forum for discussion of colloidal silver.
To join or quit silver-list or silver-digest send an e-mail message to:
[email protected] -or- [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.
To post, address your message to: [email protected]
Silver-list archive: http://escribe.com/health/thesilverlist/index.html
List maintainer: Mike Devour <[email protected]>