Mike,

The chloride is used up in the CS process in just afew seconds. It can be
seen as a white cloud coming off of the anode.afteer that point then the Ag+
ion is formed.

That is why it works.

The LVDC process makes both ionic and particulate silver. The T.E. that one
sees is reflectoins of largeparticles. Ionic silver has no T.E.

H2O2 when added to yellow silver changes it to clear.