In message <[email protected]>, Andreas Jahn wri
tes:

>you know that even a metal foil resistor can drift several 10 ppms due 
>to soldering?

You can bring that down both in PPM and time by a "degauss"
temperature-cycling sequence [+N, -N, +(N-2), -(N-2), +(N-4), -(N-4) ...]

-- 
Poul-Henning Kamp       | UNIX since Zilog Zeus 3.20
[email protected]         | TCP/IP since RFC 956
FreeBSD committer       | BSD since 4.3-tahoe    
Never attribute to malice what can adequately be explained by incompetence.