Hey guys, I am in a bit of a jam.  I have to deliver a custom rod on Sat and my Flex 
Coat is making my life difficult.  My first coats went on okay but my secon are either 
tacky or really slow to cure.  I know this is a chemical reaction vs. heat but does 
cold weather slow the process down?  It has been chilly here in Eastern, WA this week. 
 

I am going to try putting a very, very light coat on the tacky wraps tonight in hope 
that maybe my mixture was off or didn't get mixed all the way last time.  If this 
fails, any ideas on what to do?  I have read some people using products like Hard as 
Nails to force tacky Flex Coat to cure but have no experience in this.  It is a 
special Christmas present for this family to their son so I need to get it done ASAP.