Re: Stoichiometry and occupancy fractions of solid solutions

2016-12-20 Thread Wilkinson, Angus P
December 20, 2016 9:55 AM To: rietveld_l@ill.fr Subject: Re: Stoichiometry and occupancy fractions of solid solutions To increase sensitivity to partial/mixed occupation and also solve the case of 3 or more atoms in the same site (you have an infinite number of solutions that give you the same scatt

Re: Stoichiometry and occupancy fractions of solid solutions

2016-12-20 Thread Luca Lutterotti
sburg, MD 20899-8523USA > jcl...@nist.gov <mailto:jcl...@nist.gov> > (301) 975 5793 > FAX (301) 975 5334 > > From: rietveld_l-requ...@ill.fr [mailto:rietveld_l-requ...@ill.fr] On Behalf > Of Luca Lutterotti > Sent: Tuesday, December 20, 2016 9:55 AM

RE: Stoichiometry and occupancy fractions of solid solutions

2016-12-20 Thread Cline, James Dr. (Fed)
...@nist.gov<mailto:jcl...@nist.gov> (301) 975 5793 FAX (301) 975 5334 From: rietveld_l-requ...@ill.fr [mailto:rietveld_l-requ...@ill.fr] On Behalf Of Luca Lutterotti Sent: Tuesday, December 20, 2016 9:55 AM To: rietveld_l@ill.fr Subject: Re: Stoichiometry and occupancy fractions of solid sol

Re: Stoichiometry and occupancy fractions of solid solutions

2016-12-20 Thread Luca Lutterotti
To increase sensitivity to partial/mixed occupation and also solve the case of 3 or more atoms in the same site (you have an infinite number of solutions that give you the same scattering factor, both x-ray and neutrons) we are developing a combined XRD-XRF analysis. Some preliminary

Re: Stoichiometry and occupancy fractions of solid solutions

2016-12-20 Thread babaryk
> From: baba...@univ.kiev.ua <baba...@univ.kiev.ua> > Sent: Monday, 19 December 2016 9:31:29 PM > To: Othman Al Bahri > Subject: Re: Stoichiometry and occupancy fractions of solid solutions > > Dear Othman, > > General notes and precaut

Re: Stoichiometry and occupancy fractions of solid solutions

2016-12-19 Thread Leopoldo Suescun
Dear Othman, I agree with previous comments and warnings from colleagues. But regarding your specific question, you need to check the manuals for GSAS II or FULLPROF on how to setup the constraints on the site occupancies of all the atoms and sites involved. It is not sufficient to constrain

Re: Stoichiometry and occupancy fractions of solid solutions

2016-12-19 Thread Larry Finger
On 12/19/2016 09:29 AM, Cline, James Dr. (Fed) wrote: Your data is from where? I wouldn’t trust numbers from refinements as these from lab data. Jim James P. Cline Materials Measurement Science Division National Institute of Standards and Technology 100 Bureau Dr. stop 8520 [ B113 /

RE: Stoichiometry and occupancy fractions of solid solutions

2016-12-19 Thread Cline, James Dr. (Fed)
Your data is from where? I wouldn't trust numbers from refinements as these from lab data. Jim James P. Cline Materials Measurement Science Division National Institute of Standards and Technology 100 Bureau Dr. stop 8520 [ B113 / Bldg 217 ] Gaithersburg, MD 20899-8523USA