eld_l-requ...@ill.fr> on behalf of Edward Laitila <
> ealai...@mtu.edu>
> *Reply-To: *Edward Laitila <ealai...@mtu.edu>
> *Date: *Monday, May 22, 2017 at 8:19 AM
> *To: *Shay Tirosh <stiro...@gmail.com>
> *Cc: *Rietveld list <rietveld_l@ill.fr>
> *Subjec
From: <rietveld_l-requ...@ill.fr> on behalf of Edward Laitila <ealai...@mtu.edu>
Reply-To: Edward Laitila <ealai...@mtu.edu>
Date: Monday, May 22, 2017 at 8:19 AM
To: Shay Tirosh <stiro...@gmail.com>
Cc: Rietveld list <rietveld_l@ill.fr>
Subject: Re: Sample damaging d
There should be no damage but you may see a slit change in color where the
beam hits the sample, a temporary change in the color center. I suggest
running your generator at 45 kV and 35 mA you will get more intensity.
Cheers,
Ed
On Sun, May 21, 2017 at 12:21 PM, Shay Tirosh