Polyoxymethylene (POM) https://en.wikipedia.org/wiki/Polyoxymethylene ?


Nicklas Karlsson


lör 2022-10-08 klockan 12:13 -0400 skrev gene heskett:
> This is for Chris;
> 
> I printed a new carriage for an Ender 5 plus, out of PETG+CF. But
> while 
> its working right now, "cold flow" seems
> to be ruling the day.
> 
> With enough pressure on the POM rollers to contain the head, the base
> plate is warping, making the roller fit loose.
> Is there a plastic that's more stable than PETG+CF? See png from 
> OpenSCAD, the POM rollers are the 4 corner holes.
> 
> Suggestions?
> 
> Cheers, Gene Heskett.
> _______________________________________________
> Emc-users mailing list
> Emc-users@lists.sourceforge.net
> https://lists.sourceforge.net/lists/listinfo/emc-users




_______________________________________________
Emc-users mailing list
Emc-users@lists.sourceforge.net
https://lists.sourceforge.net/lists/listinfo/emc-users

Reply via email to