Is it cold or humid? You may want to try a heat lamp to get rid of the 
tackiness. 

Allie Palmer

> On Feb 11, 2019, at 11:10, Mark Jones via KRnet <[email protected]> wrote:
> 
> I am using Aeropoxy to lay up my glass. After I laid up the bottom of the 
> left stub wing and stabilizer the lay up remains tacky even after a week of 
> curing. The lay up has dried hard but just has this tackiness to the surface. 
> Any suggestions to remove the tackiness? And yes I am weighing the mix 
> according to instructions of 100/27 by weight or 3/1 volume. 
> Thanks
> 
> Mark Jones
> Oldsmar, Fl
> 
> N771MJ  “WunderBird”
> www.flykr2s.com
> [email protected]
> 
> 
> 
> _______________________________________________
> Search the KRnet Archives at 
> https://www.mail-archive.com/[email protected]/.
> Please see LIST RULES and KRnet info at http://www.krnet.org/info.html.
> see http://list.krnet.org/mailman/listinfo/krnet_list.krnet.org to change 
> options.
> To UNsubscribe from KRnet, send a message to [email protected]

_______________________________________________
Search the KRnet Archives at https://www.mail-archive.com/[email protected]/.
Please see LIST RULES and KRnet info at http://www.krnet.org/info.html.
see http://list.krnet.org/mailman/listinfo/krnet_list.krnet.org to change 
options.
To UNsubscribe from KRnet, send a message to [email protected]

Reply via email to