You have to crank the wire speed and amperage up I was using about
150Amp I think on 3mm to get adequet penetration.  To much amperage and
the weld became pourous(holes). I tried it using BOC gases Argoshield
100 (all I had), the gas must have Helium in it because it leaves a
black soot on the welds. You need pure Argon. I was able to get a decent
weld but you need practice and be careful you dont warp it. I have been
meaning to try pure Argon but my MIG's wire feed is causing me problems
at the moment. 

Craig.

> Greer wrote:
> 
> List,
> 
> Has anyone had experience with the aluminium welding wire that is
> available for mig welders?
> 
> Steve
> 
> --membersozdat-------------------------------------------------------
> OZDAT Mailing List Please Note:-
> Send (un)subscribe requests to [EMAIL PROTECTED]
> Send submissions to [EMAIL PROTECTED]
> No unauthorised redistribution of this email
> http://www.ozdat.com/ozdatonline/index.htm
> http://www.ozdat.com/ozdatonline/listindex.html
> http://www.mail-archive.com/[email protected]/
> ---------------------------------------------------------------------


--membersozdat-------------------------------------------------------
OZDAT Mailing List   Please Note:-
Send (un)subscribe requests to  [EMAIL PROTECTED]
Send  submissions to  [EMAIL PROTECTED]
No unauthorised redistribution of this email
http://www.ozdat.com/ozdatonline/index.htm
http://www.ozdat.com/ozdatonline/listindex.html
http://www.mail-archive.com/[email protected]/
---------------------------------------------------------------------

Reply via email to