I used to use MEK but you can't get that in California anymore so now
I use anhydrous isopropyl and an ultrasonic cleaner for liquid flux
and dont clean some of the hand solder.  Have been switching over to a
hot air reflow oven for the SMT which uses a no clean LF318 paste.

The simple rule is all water soluble flux must be cleaned and all
liquid fluxes should be cleaned.  Flux from no-clean wire solder does
not need to be cleaned because the.flux has gotten got enough to
incapacitate the active part of the flux.

To save on material cost I have started distilling the used alcohol at
a cost of about 25 cents a quart.