29/08/2002 22:18:44, "Dennis Saputelli" <[EMAIL PROTECTED]> wrote:
>they probably just went ISO or something :o) More likely, they're suffering from islands of resist detaching and floating around, causing 5 thou gaps wherever they land. I've certainly been asked to avoid similar features (although normally it's tracks leaving pads and looping round the side of the pad, with a few thou clearance - Specctra quite likes this tactic. Protel DRC regards these as not a problem, since they're same net, but it's a too-fine feature on the copper, and the thin section of resist, tethered only at one end, has a tendency to swing around and cut the track. Bare- board testing picks it up, but it causes rework or rejects. A rule that could spot this would be extremely handy...) Steve ************************************************************************ * Tracking #: 65DE11A4E1492F46A78D49F004B8B46E87A759C7 * ************************************************************************ * * * * * * * * * * * * * * * * * * * * * * * * * * * * * * * To post a message: mailto:[EMAIL PROTECTED] * * To leave this list visit: * http://www.techservinc.com/protelusers/leave.html * * Contact the list manager: * mailto:[EMAIL PROTECTED] * * Forum Guidelines Rules: * http://www.techservinc.com/protelusers/forumrules.html * * Browse or Search previous postings: * http://www.mail-archive.com/[email protected] * * * * * * * * * * * * * * * * * * * * * * * * * * * * * *