Hello, Does anyone have the lattice parameter for Si from NIST Standard Reference Material 640b? The PDF shows a cell edge of 5.43088 angstroms, but this is for the 640a. Can I merely use this? thank you for your help sincerely, Renata ______________________________________________ FREE Personalized Email at Mail.com Sign up at http://www.mail.com/?sr=signup
- RE: Si lattice parameter Renata Smith
- RE: Si lattice parameter Elliott, C. David
- RE: Si lattice parameter Marc Hostettler
- RE: Si lattice parameter Jim Cline