I am currently working on a rietveld refinement of CoFe2O4 using GSAS. The structural model I am using is
Site A 1/8, 1/8, 1/8
Site B 1/2, 1/2, 1/2
Oxygen site 1/4+d,1/4+d,1/4+d


On site A and B both Iron and Cobalt are present.

I am trying to create a constraint that forces the ratio of the Co:Fe to be 1:2 as well as force the fractional occupancies of each site to inverse each other . In other words percent Iron goes up percent Cobalt goes down. This part I have been able to do quite easily. I thought I was able to set up the 1:2 ratio constraint correctly but I don't believe the answer because I am getting the Cobalt on both sites to have a Fraction value of ~0.28 and the Iron fraction to = ~ 0.57. I know that I may have vacancies but I don't believe both site should be the same.

Can anyone please tell me how to set up a chemical ratio constraint either going through the EXPGUI or DOS interface?

Sincerely,

Darin Hoffman


#################################################
Darin Hoffman, TSPA
Research Intern, NPDF
Lujan Neutron Scattering Center
Los Alamos National Laboratory
e-mail: [EMAIL PROTECTED]
PH: 505-667-8704
#####################################################




Reply via email to