Title: Nachricht
Dear Angel,
 
the instrument profile is the convolution product of the source emission profile and various instrument contributions. For lab diffractometers the source emission profile has a Lorentzian type shape. Particularily for Bragg-Brentano type diffractometers, at low angles, the instrument function shape is dominated by the detector slit, which can be sufficiently approximated by a hat (impulse) function. The convolution product of the source emission profile and the detector slit contribution looks Gaussian-like, but a Gaussian is not an ideal approximation for this. At higher angles the source emission profile dominates, thats why the instrument function is more Lorentzian type.
 
I can offer you a detailed paper about this issue, please let me know if you would like to receive it.
 
Cheers,
 
Arnt
-----Urspr�ngliche Nachricht-----
Von: Angel L. Ortiz [mailto:[EMAIL PROTECTED]
Gesendet: Mittwoch, 6. Oktober 2004 12:44
An: [EMAIL PROTECTED]
Betreff: shape of the instrumental profiles

Dear colleagues:

 

Does anyone know why the instrumental profiles (instrumental resolution) are generally Gaussian for low diffraction angles, whereas turns to Lorentzian for high diffraction angles?.

 

Any advice is greatly appreciated.

 

Thanks in advance,

 

Prof. Angel L. Ortiz



**********************************************************************
Der Inhalt dieser E-Mail ist vertraulich und ausschliesslich fuer den bezeichneten Adressaten bestimmt. Wenn Sie nicht der vorgesehene Adressat dieser E-Mail oder dessen Vertreter sein sollten, so beachten Sie bitte, dass jede Form der Kenntnisnahme, Veroeffentlichung, Vervielfaeltigung oder Weitergabe des Inhalts dieser E-Mail unzulaessig ist. Wir bitten Sie, sich in diesem Fall mit dem Absender der E-Mail in Verbindung zu setzen.

The information contained in this email is confidential. It is intended solely for the addressee. Access to this email by anyone else is unauthorized. If you are not the intended recipient, any form of disclosure, reproduction, distribution or any action taken or refrained from in reliance on it, is prohibited and may be unlawful. Please notify the sender immediately.

**********************************************************************