Hi Gustavo,
Last year I started to work on identification of series of Al2O3
semiamorphous materials. Then this project was dropped. Meanwhile, I  made
brief research and my impression is that there is some chaos in the
nomenclature of the Al-oxides. Aside of this, in PDF-2 database the
situation it is also quite confusing and far away from prompt and reliable
identification. Anyway, I've got the structures of 8 Al-oxides having
different structures (2 gamma, 2 kappa, theta, sigma, eta and delta) and
simulated their powder diffraction patterns with Powder Cell for Cu k-alpha
radiation.
If this may help you, I can send to you the these 8 raw-files in x_y format.
At least they can be used as references for identification and
distinguishing of various Al-oxides.
Best regards,
Srebri

/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\
Dr. Srebri Petrov, PXRD Lab
Dept. of Chemistry, University of Toronto,
Tel/Fax: 416-978-1389
----- Original Message -----
From: "Gustavo A. Cifredo Chacón" <[EMAIL PROTECTED]>
To: <[email protected]>
Sent: Friday, January 19, 2007 12:04 PM
Subject: RE: chi alumina structure


> Thank you very much for your time,
> Excuse me, but I see that space group and cell dimensions are the same of
a
> Kappa- Al2O3 included in the ICSD. Are you sure that it is chi-Al2O3, not
> kappa? Which is the reference of the data?
>
> Thank you again.
>
>
> At 12:19 19/01/2007 +0000, you wrote:
> >  Dear Gustavo,
> >
> >the cell (space group Pna21) should be:
> >
> >4.834 x 8.3096 x  8.9353
> >
> >Structure:
> >
> >
> >  Al1    0.1778 0.8383 0.6466
> >  Al2    0.330700 0.024500 0.3775
> >  Al3    0.313800 0.350200 0.5713
> >  Al4    0.315600 0.657600 0.3734
> >  O1    0.479600 0.852900 0.4977
> >  O2    0.508500 0.508900 0.505
> >  O3    0.162700 0.163200 0.2429
> >  O4    0.154400 0.495300 0.2656
> >  O5    -0.020200 0.323100 0.5166
> >  O6    0.163800 0.841000 0.2708
> >
> >
> >I hope this will help you,
> >good luck,
> >marco
> >
> >
> >
> >-----Original Message-----
> >From: "Gustavo A. Cifredo Chacón" [mailto:[EMAIL PROTECTED]
> >Sent: 19 January 2007 11:38
> >To: [email protected]
> >Subject: chi alumina structure
> >
> >I am looking for chi-Al2O3 structural data, i.e. atomic position and
> >spacial group.
> >Any information will be wellcome.
> >
> >Thank you in advance.
> >
> >Gustavo Cifredo
> >956 016155
> >CASEM-Puerto Real
> >Universidad de Cadiz, Spain
>
> Gustavo Cifredo
> 956 016155
> CASEM-Puerto Real
> Universidad de Cadiz, Spain
>
>
>


Reply via email to