Dear Dr. Petrov,

I'm also quite interested in various phases of Al2O3 as well.  I wonder if you
have any crystallographic data for some of the phases (alpha, beta, gamma), if
not all, that you mentioned??
Thanks,
Kinson

***************************************************
Kinson C. Kam

Materials Research Laboratory,
University of California - Santa Barbara
Santa Barbara, CA. 93106.
U.S.A.

Phone:  +1 (805)893-7933
Fax:    +1 (805)893-8502
e-mail: [EMAIL PROTECTED]

***************************************************


Quoting Srebri Petrov <[EMAIL PROTECTED]>:

> Hi Gustavo,
> Last year I started to work on identification of series of Al2O3
> semiamorphous materials. Then this project was dropped. Meanwhile, I  made
> brief research and my impression is that there is some chaos in the
> nomenclature of the Al-oxides. Aside of this, in PDF-2 database the
> situation it is also quite confusing and far away from prompt and reliable
> identification. Anyway, I've got the structures of 8 Al-oxides having
> different structures (2 gamma, 2 kappa, theta, sigma, eta and delta) and
> simulated their powder diffraction patterns with Powder Cell for Cu k-alpha
> radiation.
> If this may help you, I can send to you the these 8 raw-files in x_y format.
> At least they can be used as references for identification and
> distinguishing of various Al-oxides.
> Best regards,
> Srebri
>
> /\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\
> Dr. Srebri Petrov, PXRD Lab
> Dept. of Chemistry, University of Toronto,
> Tel/Fax: 416-978-1389
> ----- Original Message -----
> From: "Gustavo A. Cifredo Chacón" <[EMAIL PROTECTED]>
> To: <[email protected]>
> Sent: Friday, January 19, 2007 12:04 PM
> Subject: RE: chi alumina structure
>
>
> > Thank you very much for your time,
> > Excuse me, but I see that space group and cell dimensions are the same of
> a
> > Kappa- Al2O3 included in the ICSD. Are you sure that it is chi-Al2O3, not
> > kappa? Which is the reference of the data?
> >
> > Thank you again.
> >
> >
> > At 12:19 19/01/2007 +0000, you wrote:
> > >  Dear Gustavo,
> > >
> > >the cell (space group Pna21) should be:
> > >
> > >4.834 x 8.3096 x  8.9353
> > >
> > >Structure:
> > >
> > >
> > >  Al1    0.1778 0.8383 0.6466
> > >  Al2    0.330700 0.024500 0.3775
> > >  Al3    0.313800 0.350200 0.5713
> > >  Al4    0.315600 0.657600 0.3734
> > >  O1    0.479600 0.852900 0.4977
> > >  O2    0.508500 0.508900 0.505
> > >  O3    0.162700 0.163200 0.2429
> > >  O4    0.154400 0.495300 0.2656
> > >  O5    -0.020200 0.323100 0.5166
> > >  O6    0.163800 0.841000 0.2708
> > >
> > >
> > >I hope this will help you,
> > >good luck,
> > >marco
> > >
> > >
> > >
> > >-----Original Message-----
> > >From: "Gustavo A. Cifredo Chacón" [mailto:[EMAIL PROTECTED]
> > >Sent: 19 January 2007 11:38
> > >To: [email protected]
> > >Subject: chi alumina structure
> > >
> > >I am looking for chi-Al2O3 structural data, i.e. atomic position and
> > >spacial group.
> > >Any information will be wellcome.
> > >
> > >Thank you in advance.
> > >
> > >Gustavo Cifredo
> > >956 016155
> > >CASEM-Puerto Real
> > >Universidad de Cadiz, Spain
> >
> > Gustavo Cifredo
> > 956 016155
> > CASEM-Puerto Real
> > Universidad de Cadiz, Spain
> >
> >
> >
>
>
>