Thanks Alan,
our first trial was:
Bergmann, J., Kleeberg, R. (1998) Rietveld analysis of disordered layer
silicates. Mat. Sci. Forum, 278-281 (1): 300-305.
Application to kaolinite at:
http://www.bgmn.de/kaolin.html
and for more disordered stuff:
http://www.bgmn.de/smectite.html
Far from beeing perfect, but sometimes working in quantification...
Reinhard
Alan Hewat schrieb:
Reinhard Kleeberg said:
There are not so much trials published to find a
working solution for practical Rietveld quantification of clays. One
would be a self-citation of a paper, so I can't do this here in the list.
A good one is :-)
Pitfalls in Rietveld Phase Quantification of Complex Samples
R. Kleeberg (2005) Microstructure Analysis in Materials Science
http://www.ww.tu-freiberg.de/mk/bht/Abstracts/kleeberg.pdf
_____________________________________________________________
Dr Alan Hewat, ILL Grenoble, FRANCE <[EMAIL PROTECTED]>fax+33.476.20.76.48
+33.476.20.72.13 (.26 Mme Guillermet) http://www.ill.fr/dif/people/hewat/
_____________________________________________________________
begin:vcard
fn:Reinhard Kleeberg
n:Kleeberg;Reinhard
org;quoted-printable:TU Bergakademie Freiberg;Institut f=C3=BCr Mineralogie
adr:;;Brennhausgasse 14;Freiberg;Sachsen;D-09596;Germany
email;internet:[EMAIL PROTECTED]
title:Dr.
tel;work:(+49) (0)3731 393244
tel;fax:(+49)(0)3731 393129
url:http://www.mineral.tu-freiberg.de/mineralogie/roelabor/
version:2.1
end:vcard