Hi,
Can anyone tell me a good source for crystal structure data for cement phases? Does anyone have ICSD numbers for alite, belite and tricalcium aluminate that they commonly use? I only found an ICDD PDF for C3A, which doesn't have an RIR. Thank you, Maria Chrysochoou, Ph.D. W.M. Keck Geoenvironmental Laboratory Stevens Institute of Technology Tel.: +1 201 216 8773 Fax: +1 201 216 8212 E-mail: [EMAIL PROTECTED]