Thank you very much man!!! We are right now making a zero background sample 
holder, with a quartz cutted 6 degrees form its c axis. 
 
We are buying Cab-O-Sil (fumed silica) as well, trying to reduce preferred 
orientation in our samples using the method of Blount and Vassilou (1979).


Subject: Re: Laboratory supplies/equipments for application of the Rietveld 
Method (quantitative analysis)Date: Wed, 26 Sep 2007 10:51:00 -0400From: [EMAIL 
PROTECTED]: [EMAIL PROTECTED] the gem dugout for zero background sample 
holders, and angle/intensity standards. 
http://www.thegemdugout.com/



On Sep 26, 2007, at 9:30 AM, Leandro Bravo wrote:
Hi All!! I´m searching for some equipments, supplies that could be useful to 
the application of the Rietveld Method (quantitative analisys) like 
zero-background sample holders, mill etc... in other words, equipments for 
sample prepare to avoid preferred orientation, microabsorption, etc.. We are 
trying to buy a Mccrone Micronizing Mill but we just can manage to contact the 
company (Mccrone Lab Supplies), any of you know other place where I can buy the 
Mccrone Mill?!?! In other hand, if we don´t buy the Mccrone Mill is there any 
other equipment that could be useful in our lab?!?! 

Receba as últimas notícias do Brasil e do mundo direto no seu Messenger com 
Alertas MSN! É GRÁTIS! Assine já!
_________________________________________________________________
Receba as últimas notícias do Brasil e do mundo direto no seu Messenger com 
Alertas MSN! É GRÁTIS!
http://alertas.br.msn.com/

Reply via email to