Martin,

The reason of your bad experience with March-Dollase can be different, however, Leonid was right. The March-Dollase is normalized, the Rietveld-Toraya not. It can be easily normalized (see for example J. Appl. Cryst. 28(1995)247-253) but in all Rietveld codes I know it is not.

Best

radovan




Martin a écrit :
Sorry to disagree. Experience tells me otherwise - the March-Dollase correction has nearly always led to poor quant results for me. It most certainly cannot be applied safely. Martin ------------------------------------------ M Vickers
Dept of Chemistry
UCL


------------------------------------------------------------------------

 > Subject: Re: Quantitative analysis
 > Date: Tue, 28 Oct 2008 02:53:20 -0700
 > From: [EMAIL PROTECTED]
 > To: [email protected]
 >
 > Dear Mario,
 >
> One more possible problem of applying preferred orientation corrections in QPA is that not all of them are normalized. For example, the March-Dollase correction is normalized and can be applied safely, but the Rietveld-Toraya correction is inapplicable to QPA as it does not preserve the scale normalization.
 >
 > Best regards,
 > Leonid
 >
 > *******************************************************
 > Leonid A. Solovyov
 > Institute of Chemistry and Chemical Technology
 > K. Marx av., 42
 > 660049, Krasnoyarsk Russia
 > Phone: +7 3912 495663
 > Fax: +7 3912 238658
 > www.icct.ru/eng/content/persons/Sol_LA
 >

------------------------------------------------------------------------
For the best free wallpapers from MSN Click here! <http://wallpapers.msn.com/?ocid=[B001MSN42A0716B]>


--
Radovan Cerny
Laboratoire de Cristallographie
24, quai Ernest-Ansermet
CH-1211 Geneva 4, Switzerland
Phone  : [+[41] 22] 37 964 50, FAX : [+[41] 22] 37 961 08
mailto : [EMAIL PROTECTED]
URL    : http://www.unige.ch/sciences/crystal/cerny/rcerny.htm


Reply via email to