Hi Nicolae! 

Of course, I refined in R-3c using your anisotropic strain model, which gave 
perfect results for both Fe2O3 and Cr2O3 up to anisotropic thermal parameters 
of all atoms: 
https://sites.google.com/site/ddmsuite/tutorials/Fe2O3-Cr2O3.png 
All that glitters is not gold, unfortunately ;) 

Best wishes, 
Leonid 

 *******************************************************
Leonid A. Solovyov
Institute of Chemistry and Chemical Technology
660036, Akademgorodok 50/24, Krasnoyarsk, Russia
http://sites.google.com/site/solovyovleonid
*******************************************************


----- Original Message -----
From: "[email protected]" <[email protected]>
To: Leonid Solovyov <[email protected]>
Cc: Lista Rietveld <[email protected]>
Sent: Sunday, May 10, 2015 3:20 PM
Subject: Re: On the   =?iso-8859-1?Q?=E 2 =80=9Ccrystallogr ap hic_good_practic 
es= E2=80=9D?=

Leonid, good point!
Molodetz! Pozdravliaiu!
Have you refined in R-3c?
Nicolae Popa
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>