Hi,

 

Sorry for that blank email...

Since times are to old stories about the Rietveld method, I first
heard about it in 1975-76 during my "3ème cycle" thesis in D. Grandjean
laboratory, Rennes, France, under the direction of D. Louër. The thesis 
was about profile-shapes broadening due to powder small grain size.
http://www.cristal.org/rapport/Le-Bail-These-3eme-Cycle.pdf

I did not use the Rietveld method at that time but I remember that
a Fortran version was in tests there, probably one of these 27 copies
distributed by Hugo Rietveld himself to institutes all over the world.
http://home.wxs.nl/~rietv025/Rietveld%20Method.docx

My profile shapes were quite Lorentzian and there was considerable
anisotropic broadening, something not yet accountable by the Rietveld
method at that time focused on Gaussian peak shapes.

I was not back about the Rietveld method before the XIII IUCr Congress,
1984, Hamburg, where I proposed a way to undertake such X-ray complex
shapes: "The Rietveld method using an experimental profile convoluted 
by adjustable analytical function". This was the ARIT software later
used in 1987 for intensities extraction purposes by iterating the
Rietveld decomposition formula, leading to many SDPDs (Structure
Determination by Powder Diffractometry).
http://cristal.org/mespapiers-PDF/1984/1984-Rietveld-a31186.pdf
http://www.cristal.org/arit.html

Best,

 

Armel

 

PS- Better to write your own story clearly yourself before to leave the planet,

even if nobody apparently read it.

http://www.cristal.org/iniref/lbm-story/

 

 

 

 

 

 
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to