It takes about 2-3 hours to go to from 28 to 6v after which it starts making "sludge" I am thinking of buying my own distiller so that I can control the process better.
I have been brewing only 1 liter batches. I found a 300g coffee jar ideal. Plus it was a glass jar. I cannot increase the width of the electrodes any further than 3.5cm as I have mounted them on the coffee jar lid. Which doesn't give me much real estate after the motor on top. I understand that the silvergen SG6 has it's electrodes 2cm apart and uses 1 ma. ( I remember from a trem's post) I have been wiping the electrodes every 20 mins. The cathodes get black fairly quickly. Although things have improved by using 3 anodes. And distancing the electrodes further to 3.5cm. They seem to make the brew more cleanly. I have run out distilled water. So I will not be able to tweak the setup until then. Also may I ask what voltage and current are you using for your setup? Sent from my iPhone On 6 Jun 2011, at 23:57, Neville Munn <[email protected]> wrote: > Hi Asif, > > I don't believe you mentioned how long your brew process goes, but here's a > couple of things I'd be looking into: > > a) Taking the electrodes out to 4cm apart. > b) Using a larger volume brew vessel for that dimension electrodes. I brew a > litre or more at a time using electrodes shorter than yours {between 8cm and > 10cm depending on which of my units I use on the day}. My electrodes are 3mm > dia tho. > c) Remove the electrodes at regular timed intervals to wipe them clean {if > you think they need it or not} before resubmerging them. > > Sparklies in the water?...I've noticed that some DW I purchase {only an El > Cheapo brand} shows some sparklies upon using laser pointer straight from the > bottle. I have also seen microscopic bits of 'fluff?' or fibre, or whatever > may be in the air on the day I brew become evident in the water after a > couple days in storage {I store in sealed containers}. I believe these give > the illusion of settlement due to some silver 'attaching?' to these > microscopic bits of 'stuff?' present in the DW, or which has entered the > water from the air during my brew process {I brew in an open top vessel}. > > Just a few things I'd be looking at if it were me. > > N. > > From: [email protected] > To: [email protected] > Date: Mon, 6 Jun 2011 19:27:43 +0100 > Subject: CS>question regarding CS production > > -- The Silver List is a moderated forum for discussing Colloidal Silver. Rules and Instructions: http://www.silverlist.org Unsubscribe: <mailto:[email protected]?subject=unsubscribe> Archives: http://www.mail-archive.com/[email protected]/maillist.html Off-Topic discussions: <mailto:[email protected]> List Owner: Mike Devour <mailto:[email protected]>