Yesterday I made a 16 oz batch of CS using virtually the same methods I have used before.

In the past, I have used the 27 volt LVDC generator, with 2 small 12 volt batteries connected in series. This would be 51 VDC, virtually the same as the telephone generator I am testing.

I used no saline.  Added about 1 oz CS from a previous batch.  ( 16 oz batch )

The color is lemon, or pale yellow and tastes bitter. The time on this batch was about 3.5 hours.

After determining that the batch was ok, ( or so I thought ) I used a four ounce bottle and mixed 50-50 with DMSO for a fungicide treatment to be used for toenail fungus.

Even thru the brown bottle, I could see strange things happening. Plus a noticable warming effect was noticed. The bottle did not get hot, but it was more than slightly warm. Medium warm, but not hot.

After a time, it cooled off.

The bottle was a 4 ounce dropper bottle with the rubber bulb. No glass or plastic dropper tube was installed in the rubber bulb. The bottle was about 90% full.

12 hours later, the bottle was about 20 % full. The top was screwed on with a reasonable tension.

Can anyone offer and facts as to what happened?

I have 16 ounces of the CS and more of the DMSO. Should I see if this will happen again?

Wayne


--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: [email protected] -or- [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]
Silver-list archive: http://escribe.com/health/thesilverlist/index.html
List maintainer: Mike Devour <[email protected]>