Wayne,
A characteristic of DMSO is that it gives off heat when diluted with
water. I can't explain the loss of volume.
regards, 
Tony

Wayne Fugitt wrote:
> 
> Yesterday I made a 16 oz batch of CS using virtually the same methods I
> have used before.
> 
> In the past, I have used the 27 volt LVDC generator,  with 2 small 12 volt
> batteries connected in series.
> This would be 51 VDC, virtually the same as the telephone generator I am
> testing.
> 
> I used no saline.  Added about 1 oz CS from a previous batch.  ( 16 oz batch )
> 
> The color is lemon, or pale yellow and tastes bitter.  The time on this
> batch was about 3.5 hours.
> 
> After determining that the batch was ok, ( or so I thought )  I used a four
> ounce bottle and mixed 50-50 with DMSO for a fungicide treatment to be used
> for toenail fungus.
> 
> Even thru the brown bottle, I could see strange things happening.  Plus a
> noticable warming effect was noticed.
> The bottle did not get hot, but it was more than slightly warm.  Medium
> warm, but not hot.
> 
> After a time, it cooled off.
> 
> The bottle was a 4 ounce dropper bottle with the rubber bulb.  No glass or
> plastic dropper tube was installed in the rubber bulb.   The bottle was
> about 90% full.
> 
> 12 hours later, the bottle was about 20 % full.   The top was screwed on
> with a reasonable tension.
> 
> Can anyone offer and facts as to what happened?
> 
> I have 16 ounces of the CS and more of the DMSO.  Should I see if this will
> happen again?
> 
> Wayne
>



--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: 
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]
Silver-list archive: http://escribe.com/health/thesilverlist/index.html
List maintainer: Mike Devour <[email protected]>