Mike, I know that you mean well, but you cannot account for the fact that with the good W-M DW the conductance may be 31.6 and the measure PPM with a spect is 29.5 or the sample submited for TEM had conductance of 12 uS/cm and a 8.96 ppm.
With the new WM DW that is not the case, Cond. = 78 uS/cm and PPM = 17.6. I have run eight 2 gallon lots and that same differences exist. Trem gave some good advice, and my personal opinion as a EE with many tail feathers (visit my web www.hvacsilver.com), why do your "fart" around with a salt test and exact equations with dubious data??? "Ole Bob" -- The silver-list is a moderated forum for discussion of colloidal silver. Instructions for unsubscribing may be found at: http://silverlist.org To post, address your message to: [email protected] Silver-list archive: http://escribe.com/health/thesilverlist/index.html List maintainer: Mike Devour <[email protected]>