I think it could be the heated DW which is the trouble. Wonder also what
you heat the DW in? could it be picking up contamination from whatever
container you heat it in? Is there some reason you need to make your CS
that fast?
For what its worth I never scrub my electrodes, it's a waste of silver.
I just wipe them off with a white paper napkin or paper towel, or even
plain toilet tissue.
sol
Pat wrote:
. Does anyone here heat the distilled water to almost boiling first?
I was told to do that by the guy who first told me about CS and he's
been making it about 8 years I think. It sure does make it finish faster.
Pat
------------------------------------------------------------------------
Yahoo! DSL
<http://pa.yahoo.com/*http://us.rd.yahoo.com/evt=37474/*http://promo.yahoo.com/broadband/%20>
Something to write home about. Just $16.99/mo. or less
------------------------------------------------------------------------
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.1.371 / Virus Database: 267.14.9/217 - Release Date: 12/30/2005
--
Whenever you find you are on the side of the majority, it is time to pause and reflect. Mark Twain
--
The Silver List is a moderated forum for discussing Colloidal Silver.
Instructions for unsubscribing are posted at: http://silverlist.org
To post, address your message to: [email protected]
Address Off-Topic messages to: [email protected]
The Silver List and Off Topic List archives are currently down...
List maintainer: Mike Devour <[email protected]>