Thank every one for the propositions.
Find here after the result of a test (vaseline + n-heptane)
http://perso.univ-lemans.fr/~fgouten/Transmission_Tricks
Best Regards, François
Le 08/02/2017 13:35, François Goutenoire a écrit :
Dear Rietveld users,
We are currently using transmission flat sample on our diffractometer.
To prepare the transmission flat sample we are using mylar 15microns
or kapton. We put the sample between 2 mylar foils.
I would like to know if there is some tricks in order to nicely put
the powder in the center of the circular sample older and if there is
also some tricks in order to avoid electrostatic problems.
Thank you very much in advance,
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list<alan.he...@neutronoptics.com>
Send commands to<lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
--
*********************************************************************************************
Pr. Francois GOUTENOIRE
e-mail: francois.gouteno...@univ-lemans.fr
Tel: 02.43.83.33.54
FAX: 02.43.83.35.06
Département des Oxydes et Fluorures
Institut des Molécules et des Matériaux du Mans
IMMM - UMR CNRS 6283
Université du Maine - Avenue Olivier Messiaen
F-72085 Le Mans Cedex 9
FRANCE
*********************************************************************************************
Formation Rietveld CNRS
https://cnrsformation.cnrs.fr/stage.php?stage=17082
Formation SASX CNRS
https://cnrsformation.cnrs.fr/stage.php?stage=17228
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <alan.he...@neutronoptics.com>
Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++