How about larger pipes on the mounts?  Like a 2-3"?  Sector Frames?

I know you do injection molding for your antennas, have you ever thought
about doing NEMA style boxes?

Just some ideas to throw around...

Regards,
Chuck

On Thu, Jan 22, 2015 at 4:14 PM, <ch...@wbmfg.com> wrote:

>   Thanks, wish I could take total credit.  The quality of the hot dip
> galvanize job is a bit out of our hands.  The amount of dross on the pot,
> temperature of the day, mix of zinc and other things as well as freshness
> of the pickling tank and pickling time all go into the quality of the
> galvanization and we farm that out to a local company.  We have been
> working on the fit and inspection.
>
> I appreciate the note, we do try.  And we are always up for making other
> hot dipped tower products.  Anyone want us to add to the product line, let
> me know and I will see if I can improve on the price or performance on any
> other product out in the world.  I prefer to do custom stuff nobody else
> does, but I am not above knocking off something if I can offer something in
> the way of design improvement or cost reduction.
>
>  *From:* Josh Luthman <j...@imaginenetworksllc.com>
> *Sent:* Thursday, January 22, 2015 1:25 PM
> *To:* af@afmug.com
> *Subject:* [AFMUG] WBMFG quality going up! Buy buy buy!
>
>  Props to WB for improving their MTOWs.  Most notably the cleaner
> galvanizing and the hardware fitting together perfectly.  Not a huge
> difference since these products have already been great, but the quality
> bonus is noticeable and appreciated!
>
> Josh Luthman
> Office: 937-552-2340
> Direct: 937-552-2343
> 1100 Wayne St
> Suite 1337
> Troy, OH 45373
>