WOW!

They look factory new :-)

And ouch, it really stains your worktable i can see;-)

Wondering how that coating would look on my IN-8-2 in the bedroom clock....

// Per.


On 26/10/2011, at 17.07, MichaelB wrote:

> Here are some Pics. I used another French product called Pebeo
> Vitrail, Orange #16 color. It's available on line from most higher end
> Art supply houses. Applied it using a cheap shot glass. Worked really
> well and the end result is really pretty nice!
> 
> 
> http://www.badnixie.com/Web_Files/IMG_2275.JPG
> http://www.badnixie.com/Web_Files/IMG_2276.JPG
> http://www.badnixie.com/Web_Files/IMG_2279.JPG
> 
> Here's Jeff's NixiChron with some souped up IN-18's:
> http://www.youtube.com/watch?v=xVj8MCtPX0s
> 
> 
> On Oct 26, 3:56 am, Per Jensen <[email protected]> wrote:
>> Pictures !!
>> 
>> I want to see the dipped tubes :-)
>> 
>> // Per
>> 
>> Den 26/10/2011 kl. 10.14 skrev Nick <[email protected]>:
>> 
>> 
>> 
>> 
>> 
>> 
>> 
>>> The reason I was asking about photographing VFDs is that I've recently
>>> been playing with re-coating tubes whose original coating is in poor
>>> condition or is not the wanted colour.
>> 
>>> John Smout, as always, was a fount of knowledge on these matters and
>>> suggested FEV (French Enamel Varnish) - much used in the stage &
>>> screen industries - essentially this is French Polish with a ready-
>>> mixed in stain. The solvent for FEV (and French Polish) is methylated
>>> spirits.
>> 
>>> I therefore ordered 250ml of Mauve from
>>> http://www.goldleafsupplies.co.uk/acatalog/V_French_Enamel_Varnish.html.
>> 
>>> The subject tube was cleaned with methylated spirits and the tube held
>>> upside-down in a suitable socket. I then dipped the tube into the FEV
>>> up to the desired line, then withdrew it and hung it up to dry (about
>>> 30 minutes). The coat was blemish-free and completely even with a
>>> uniform colour depth. Granted, the tube I was testing this on had a
>>> nipple which acts as a focus for drips draining off, but I see no
>>> reason why this wouldn't work with smooth-topped tubes.
>> 
>>> After a few hours the coating is tough and stands a reasonable amount
>>> of man-handling - the colour can be deepened by applying multiple
>>> coats - the whole new coating can of course be removed with the FEV
>>> solvent - methylated spirits again.
>> 
>>> FEV is available in a very wide range of colours - it is expensive,
>>> but you don't need much. I had a whole bunch of rather rare VFDs with
>>> damaged coatings - now they are like new.
> 
> -- 
> You received this message because you are subscribed to the Google Groups 
> "neonixie-l" group.
> To post to this group, send an email to [email protected].
> To unsubscribe from this group, send email to 
> [email protected].
> For more options, visit this group at 
> http://groups.google.com/group/neonixie-l?hl=en-GB.
> 

-- 
You received this message because you are subscribed to the Google Groups 
"neonixie-l" group.
To post to this group, send an email to [email protected].
To unsubscribe from this group, send email to 
[email protected].
For more options, visit this group at 
http://groups.google.com/group/neonixie-l?hl=en-GB.

Reply via email to