Hi Mike,
   The glass coloring just filter what the tube emits.
If the wavelength that the filters let pass is emitted by the tube
(like green for green-turquoise VFDs, red for Nixies) then the
coloring will enhance the contrast. And look good.
The filters will not change the color of the light emitted, like
making a Nixie to be seen as emitting green light.

Regards

On Oct 26, 9:51 am, mike <[email protected]> wrote:
> what color can the tubes be made to glow
>
>           thanks
>                            mike
>
> On Oct 26, 3:56 am, Per Jensen <[email protected]> wrote:
>
>
>
>
>
>
>
> > Pictures !!
>
> > I want to see the dipped tubes :-)
>
> > // Per
>
> > Den 26/10/2011 kl. 10.14 skrev Nick <[email protected]>:
>
> > > The reason I was asking about photographing VFDs is that I've recently
> > > been playing with re-coating tubes whose original coating is in poor
> > > condition or is not the wanted colour.
>
> > > John Smout, as always, was a fount of knowledge on these matters and
> > > suggested FEV (French Enamel Varnish) - much used in the stage &
> > > screen industries - essentially this is French Polish with a ready-
> > > mixed in stain. The solvent for FEV (and French Polish) is methylated
> > > spirits.
>
> > > I therefore ordered 250ml of Mauve from
> > >http://www.goldleafsupplies.co.uk/acatalog/V_French_Enamel_Varnish.html.
>
> > > The subject tube was cleaned with methylated spirits and the tube held
> > > upside-down in a suitable socket. I then dipped the tube into the FEV
> > > up to the desired line, then withdrew it and hung it up to dry (about
> > > 30 minutes). The coat was blemish-free and completely even with a
> > > uniform colour depth. Granted, the tube I was testing this on had a
> > > nipple which acts as a focus for drips draining off, but I see no
> > > reason why this wouldn't work with smooth-topped tubes.
>
> > > After a few hours the coating is tough and stands a reasonable amount
> > > of man-handling - the colour can be deepened by applying multiple
> > > coats - the whole new coating can of course be removed with the FEV
> > > solvent - methylated spirits again.
>
> > > FEV is available in a very wide range of colours - it is expensive,
> > > but you don't need much. I had a whole bunch of rather rare VFDs with
> > > damaged coatings - now they are like new.

-- 
You received this message because you are subscribed to the Google Groups 
"neonixie-l" group.
To post to this group, send an email to [email protected].