>(I am not sure what other Rietveld programs allow this as well?)
WinMProf uses the phenomenological Stephens model of anisotropic
peak broadening. Much less expensive than TOPAS.
http://pecdc.univ-lemans.fr/WinMProf/WinMProf.htm
GSAS, free as well, was the first to apply it.
Fullprof used a similar but incomplete approach before Stephens.
First use of elements of spherical harmonics for anisotropic line
broadening in the Rietveld method in the years 1986-7. See for instance
P. Thompson, J.J. Reilly and J.B. Hastings, J. Less Common Metals,
129 (1987) 105-114.
Best,
Armel Le Bail
http://sdpd.univ-lemans.fr/course/