Dear Ramadas,
Your problem is that your Si atoms are related by equivalent positions
to the ones you need for your restraint. You need to get all of them
within bonding distance of each other by transforming them via the
symmetry operators. Then angle restraints will be easy. Run disagl to
get equivalent positions for the atoms in the angles you want to
restrain.
Bob Von Dreele

R.B. Von Dreele
IPNS Division
Argonne National Laboratory
Argonne, IL 60439-4814



-----Original Message-----
From: Ramadas Sunil Pophale [mailto:[EMAIL PROTECTED] 
Sent: Tuesday, December 18, 2007 4:05 PM
To: [email protected]
Subject: bond angle restraints


Dear GSAS users,

May be a tad trivial question. I am refining a structure with 5 SI
atoms. I want to include soft restraints, both bond length and bond
angle. I can add the bond length restraints easily using expedt.
However, run into a small problem while trying to add bond angle
restrains.

The program asks me to include sequence number for the atoms involved.
Since there are 5 I try combinations such as 1-2-3 etc. I get a message
saying the bond length of 1-2 is 13 A > 2 A so restraint cannot be
added. I know I can change the limit from 2 A to something else, but
still this is confusing because when I added the bond restraint, the
distance between 1 and 2 was shown to be around 3.147, closer to the
expected 3.1 A for Si-Si bond. So I was confused as to why it would be
shown to be ~ 13 A the second time around.

Thanks in advance for your help.

Happy holidays :-)

Ramdas.


Reply via email to