Hello, I have just recently seen the benefits of colloidal silver with some 
warts that I HAD.  Therefore... I have started to make my own cs at home.  I am 
not sure if I am successful with my attempts.
I made my generator from some instructions I found on the net. (made with 
simple parts from Radio Shack). After using pure steam distilled water, and 
after about 5 different attempts, varying timing and water temperature, I am 
not sure what I have come up with! I have read so many different variations on 
procedures for making it, I am not sure which to believe is the best or correct 
way to go.  I suppose that I would like to obtain a clear (not cloudy) solution 
that is colorless or slightly yellow and has no more than 5 ppm. I am really 
not interested in making gallons at a time - just a few ounces at a time.  I do 
not live in an area where I have access to a testing lab so that I might get my 
cs tested for ppm; and is this entirely necessary anyway?  Will there be 
variations each time you make a "batch" or will the properties be consistent if 
performed the same way each time?   On the first try, I used 8 oz. room temp 
(72 degrees) water at 18 minutes.  It turned out clear colored but a little 
cloudy and tasted very "dirty" and not mineral tasting at all.  Next attempt 
was 8 oz. with 90 degrees for 8 minutes with virtually the same results.  Next 
I used 8 oz. at room temp and let go for 40 minutes - there was much yellow 
clouding and the silver wires were very oxidized - the solution was very cloudy 
and with an extremly dirty bitter taste. Also after this I noticed large 
pitting holes on the silver wire.  On the next try, I boiled the water, 16 oz. 
and let it run for a period of 14 minutes.  I then got a very clear solution 
that was very light yellow but it still had a slightly dirty bitter taste.

My first (and only) experience with cs was a purchase from a health food store. 
 The solution was slightly yellow and perfectly clear and had such a slight 
taste of minerals.  The stuff that I have made so far does not have a mineral 
taste but a dirty bitter  (as if you had soaked some grimy oily car engine 
bolts in a bucket of water) taste.  Is this because I had too much oxidation 
from the silver?  I know my water must be good; it is steam distilled so it 
should not have minerals.  My wires are about 16 gauge.

Are there any standard methods for making cs at home using the home made 
generator; as far as quantities, water temp and activation time? or is it 
simply left up to the individual to try to reach some uniformity.  Thanks for 
any help that anyone can provide.

Kathy