From: [email protected]
Subject: Re: CS>HVAC CS
Resent-From: [email protected]
Resent-Date: Sat, 27 Jul 2002 18:53:22 -0700

In a message dated 7/27/2002 9:35:07 PM Eastern Daylight Time,
[email protected] writes:


I have a LVDC generator which I use to produce 44oz batches -- each batch is
clear,
and stays that way, until it is all gone - about 3 weeks.
********************

To my understanding, it must be low PPM.  The point I was trying to make is,
hvac makes a strong product that is still clear.  YOu can't do that with DC
I don't think.  Either way, it's the high voltage, sometimes 15000 volts,
that causes a stronger bond and smaller particles.  To my understanding.

What DC unit are you using?  Maybe there is something I do not know and
would like to.  Thanks.
****************************
I have a Silvergen SG6 --- "Our generators produce particle sizes ranging
from .0006 to .005..."
microns, now that's small!!    Check out :

http://silvergen.com

there are electron microscope pictures of  CS product.

Jack