Thank every one for the propositions.
Find here after the result of a test (vaseline + n-heptane)
http://perso.univ-lemans.fr/~fgouten/Transmission_Tricks
Best Regards, François
Le 08/02/2017 13:35, François Goutenoire a écrit :
Dear Rietveld users,
We are currently using transmission flat
velaga <vsrihari_k...@yahoo.co.in>
Sent: Thursday, February 9, 2017 12:08:57 AM
To: François Goutenoire; rietveld_l@ill.fr
Subject: Re: Tricks for transmission sample preparation between foils
Dear Pr. Francois GOUTENOIRE,
In case of kapton tape there is a chance of getting diffraction peak at l
Dear Pr. Francois GOUTENOIRE,
In case of kapton tape there is a chance of getting diffraction peak at low
angle, I prefer to use magic scotch tape.
Some times to avoid the background from this tape as well, I use small punch in
the thick paper card and pack the material in that hole for
the results?
Thanks in advance,
Gili
-Original Message-
From: rietveld_l-requ...@ill.fr [mailto:rietveld_l-requ...@ill.fr] On Behalf Of
Fran?ois Goutenoire
Sent: Wednesday, February 08, 2017 2:35 PM
To: rietveld_l@ill.fr
Subject: Tricks for transmission sample preparation between foils
Dear Rietveld users,
We are currently using transmission flat sample on our diffractometer.
To prepare the transmission flat sample we are using mylar 15microns or
kapton. We put the sample between 2 mylar foils.
I would like to know if there is some tricks in order to nicely put the
powder