[EMAIL PROTECTED] wrote:

Well time to eat Crow.

While on the phone to Dennis. This is a 8 hour a week habit right now...

I had him do a NiCd electrolyte splash test.  He dumped some Koh onto a
slab of Aluminum. First Nothing, then about 30 seconds later, small
bubbles. Definatley liberating Hydrogen.
        That means that the cases I have are NOT Aluminum. What they are is
still a mystery. Most likely Stainless. NON magnetic, non Rusting, funny
Alum color but heavier. NOT grey like Titanium. 
        I would now test the Steel to see what it does, and also Stainless to
see the effect.

The Alum and KOH is the Draino test. It better fizz.

-- 
Rich Rudman
Manzanita Micro
www.manzanitamicro.com
1-360-297-7383,Cell 1-360-620-6266