Magnesium perhaps? Rich Rudman wrote:
>[EMAIL PROTECTED] wrote: > > >Well time to eat Crow. > >While on the phone to Dennis. This is a 8 hour a week habit right now... > >I had him do a NiCd electrolyte splash test. He dumped some Koh onto a >slab of Aluminum. First Nothing, then about 30 seconds later, small >bubbles. Definatley liberating Hydrogen. > That means that the cases I have are NOT Aluminum. What they are is >still a mystery. Most likely Stainless. NON magnetic, non Rusting, funny >Alum color but heavier. NOT grey like Titanium. > I would now test the Steel to see what it does, and also Stainless to >see the effect. > >The Alum and KOH is the Draino test. It better fizz. >