In doing a little reading. My boat is in fresh water, in which case zinc is not 
reccomended. Folks are talking about magnesium. Should I even worry about it in 
the great lakes for a boat that spends 4 months in the water?

Derek.0





________________________________
From: "Judith Blumhorst, DC" <[email protected]>
To: [email protected]
Sent: Wednesday, June 10, 2009 6:53:13 PM
Subject: Re: [IC27A] Zincs





Ditto what Bruce says.
 
I've got 2 streamlined collar anodes on the prop shaft and a 3 or 4" diameter 
"rudder" anode on the strut.
 
The rudder anode looks like two discs, one on each side of the strut.  The 
discs are attached with a bolt through the strut.)
  
Don't obstuct the water flow into the cutlass bearing when you attach the shaft 
anodes.  Be sure to leave a 1/4" or 1/2" between the shaft anode and the 
cutlass bearing.  
 
On average, they last about 8 months, depending on what boats move into the 
area....  the diver checks them every 4 months and replaces them as indicated.  
 
I'd recommend the anodes that erode from the outside surface inward.   It's 
easier to tell when they're almost consumed.  They have a small percentage of 
cadmiumin added to the alloy.  
 
Fair winds,
Judy B





________________________________
 From: Bruce Horne <bho...@ecieng. com>
To: ic...@yahoogroups. com
Sent: Wednesday, June 10, 2009 2:39:21 PM
Subject: RE: [IC27A] Zincs


Hello:
I have one on the shaft but I’m thinking about putting one on the strut also.  
It’s getting pock marked.    I’m thinking the flat kind that power boaters use 
.  I could drill and tap a hole to attach it.  The rubber inside the cutlass 
bearing electrically isolates the strut from the shaft so the shaft zinc can’t 
protect the strut.  The bronze thru-hulls would be protected by a bonding wire, 
although I don’t have one and they are in great shape for an old boat (and 
Nigel Calder doesn’t recommend bonding the thru-hulls - he states they will 
actually deteriorate faster if attached to a bonding wire.
 
From:ic...@yahoogroups. com [mailto:IC27A@ yahoogroups. com] On Behalf Of Derek 
Atkin
Sent: Wednesday, June 10, 2009 5:04 PM
To: ic...@yahoogroups. com
Subject: [IC27A] Zincs
 





What is the usual compliment of zincs on a C27? I checked catalina direct that 
they didn't have much in the way of parts. I want to be sure I am not missing 
any when I splash the boat.

Thanks

Derek.
#4297
79 C27

________________________________
 
No viruses found in this incoming message
Scanned by iolo AntiVirus 1.5.6.4
http://www.iolo. com 

________________________________
 No viruses found in this outgoing message
Scanned by iolo AntiVirus 1.5.6.4
http://www.iolo. com 
   


      

Reply via email to