I'm having this discussion at the moment with a neon specialist - the
Penning mixture varied, as did the baking, pressure, type of glass &
level of Hg doping. Some tubes had getters which only fire once, so
refilling, which is what I'm investigating, is non trivial. Its a
completely different process to that used for neon signs...

I have a few potentially extremely nice tubes that have out-gassed
(nipple broken etc) and I'm looking at restoring these...

Nick

On Oct 29, 9:58 am, Jens Boos <[email protected]> wrote:
> Hi folks,
>
> I was wondering, what exact gas mixture is used in Nixie tubes? I
> heard about 2% Argon in Neon, would that work?
>
> Regards,
> Jens

-- 